New development( the sodium silicate and carbonic acid 納s
its gather the thing totally)
|
| 1. The fleetness fuses( about 50, need about tradition
90 second~200 second) |
| 2. Melt 100% completely( tradition of fuse about
90%,10% is sunk to accumulate in fabric) |
| 3. Provide the high alkalinity, reach good wash
the result clearly. |
| 4. The fleetness also does away with the calcium,
magnesium heavy metals effectively. |
| 5. Grain form appearance, the pole is applicable
to the powder body formulation. |